MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Milliken® RenewWrap™ CF300 Carbon Fiber Fabric
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: RenewWrap™ CF300 is a dry, unidirectional carbon fiber fabric made with high strength, standard modulus carbon fibers. RenewWrap CF300 fabrics, along with RenewWrap Saturant are used to strengthen or retrofit existing concrete and masonry structures.

Features and Benefits:

  • Lightweight, flexible, high strength fabric can be wrapped around and externally bonded to structural elements
  • Easy to impregnate using wet or dry lay-up methods
  • EZ-Measure™ system for quick measurement of fabric lengths and alignment of fabrics in field and in witness panel fabrication.
  • EZ-Slit™ system enabling accurate, rapid, and clean slitting of fabrics to desired widths.
  • Non-corrosive
  • Minimal aesthetic impact

Information provided by Milliken®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 20.0 mil
Coating Weight 300 g/m²
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 830 MPa
Elongation at Break 1.1 %
Modulus of Elasticity 77.0 GPa
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 66.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 60.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Milliken® VelaCarb 335 Carbon Fiber Fabric
Fibre Glast 530 Plain Weave Carbon Fiber Fabric
Solvay CYCOM® 950-1 Epoxy Prepreg with 42%-T800-Plain Weave-200 GSM
Milliken® VelaCarb 600 Carbon Fiber Fabric
Solvay CYCOM® 2040 Epoxy Prepreg Fabric with 6KM46J-2X2T-200

PMILLIK050 / 195021

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.