MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Borealis Borcoat" EB133E-1199-LT Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Borcoat EB133E-1199-LT is an elastomer modified compound, based on a polypropylene copolymer. It has excellent low temperature impact resistance. The product is colored white. It includes a combination of stabilizers to ensure long-term thermal stability. The product is supplied in pellet form.

Applications: Borcoat EB133E-1199-LT is recommended as a top coat for multilayer PP systems and thermal insulation used in: Steel Pipe Coating

Specifications: Borcoat EB133E-1199-LT is intended to fulfil following National and International standards, when appropriate industrial manufacturing standard procedures are applied and a continuous quality system is implemented and when used in combination with Borcoat™ BB122E-LT and a compatible powder epoxy. ISO 21809-1; DIN 30678; NF A49-711; Gazprom 2-2.2-178-2007

Borcoat EB133E-1199-LT is intended for design temperatures between -20°C and +110°C and tailored for low temperature handling, transportation and installation.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.915 g/ccISO 1183-1, Method A
ESCR 10% Igepal® >= 5000 hour
@Temperature 50.0 °C
ASTM D 1693-A
Oxidative Induction Time (OIT) >= 40.0 min
@Temperature 220 °C
ISO 11357-6
Melt Flow 1.20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
Storage Temperature <= 50.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60.0
@Time 1.00 sec
ISO 868
Tensile Strength, Yield 22.0 MPa50 mm/min; ISO 527-2
Elongation at Break >= 400 %50 mm/min; ISO 527-2
Elongation at Yield 13.0 %50 mm/min; ISO 527-2
Tensile Modulus 1000 MPa1 mm/min; ISO 527-2
Charpy Impact, Notched 4.00 kJ/m²
@Temperature -30.0 °C
ISO 179
 5.00 kJ/m²
@Temperature -20.0 °C
ISO 179
 60.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 135 °C
@Load 1.02 kg
A50; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 220 °CCylinder
Die Temperature 200 - 240 °C
Melt Temperature 200 - 240 °C
Head Temperature 210 - 220 °C
 
Descriptive Properties
Moisture Content<500 ppmKarl Fischer-titration, ISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9622 / 322979

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.