TRA-BOND 400-5 adhesive is a general purpose non-conductive epoxy. It combines the properties of a moderate work life with the ability to cure rapidly at temperatures as low as 60°C. Having a relatively low viscosity, TRA-BOND 400-5 adhesive is well suited for use in wet coil winding applications. Information provided by Tra-Con Inc. |