MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsui TPX® MBZ230 Methylpentene Copolymer, Filled, Opaque Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polymethylpentene (PMP)

Material Notes: TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equipment, laboratory ware, small appliances, ovenware, baking cartons, release paper, wire and cable coating, and a number of industrial uses. TPX is manufactured and marketed solely by Mitsui Chemicals, Inc.

Applications:

  • Injection Molded Items:
    • Blood test cells
    • Medical instruments
    • Laboratory ware
    • Coffee maker parts
    • Cosmetic containers
  • Extrusion Molded Items:
    • Sight glass (pipes, sheets)
    • Baking cartons (food containers)
    • Release paper
    • Wire and cable coating
    • Films

Molding Method:

  • Injection

Information provided by Mitsui.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D1505
Water Absorption 0.11 %24 hours; ASTM D570
Linear Mold Shrinkage 0.017 cm/cmMPC method, MD
Linear Mold Shrinkage, Transverse 0.014 cm/cmMPC method
Melt Flow 30 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 90ASTM D785
Tensile Strength at Break 16.7 MPa5mm/min; ASTM D638
Tensile Strength, Yield 23.5 MPa5mm/min; ASTM D638
Elongation at Break 25 %MPC method, 5mm/min
Modulus of Elasticity 1.86 GPaTangent; ASTM D790
Flexural Strength 38.2 MPaASTM D790
Izod Impact, Unnotched (ISO) 14.7 kJ/m²
@Thickness 2.00 mm,
Temperature 20.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 240 °CMPC Method
Deflection Temperature at 0.46 MPa (66 psi) 110 °CASTM D648
Vicat Softening Point 175 °CASTM D1525
 
Descriptive Properties
AppearanceWhite Opaque

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsui TPX® RT18 XB Methylpentene Copolymer
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade
Mitsui TPX® MX004 Methylpentene Copolymer
Mitsui TPX® MX002 Methylpentene Copolymer
Mitsui TPX® DX820 Methylpentene Copolymer

PMIT051 / 53232

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.