MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Omni Plastics OmniLon™ PA6 Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Injection molding grade; values are based on natural or black materials unless otherwise noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccASTM D792
Linear Mold Shrinkage 0.011 - 0.016 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.011 - 0.016 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 73.0 MPaASTM D638
Elongation at Break 40 %ASTM D638
Flexural Strength 107 MPaASTM D790
Flexural Modulus 2760 MPaASTM D790
Izod Impact, Notched 53.0 J/m
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 177 °C
@Thickness 3.17 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C
@Thickness 3.17 mm
ASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
Omni Internal Testing
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 450 - 520 °F
Middle Barrel Temperature 460 - 520 °F
Front Barrel Temperature 460 - 520 °F
Nozzle Temperature 480 - 540 °F
Melt Temperature 450 - 520 °F
Mold Temperature 80.0 - 180 °F
Drying Temperature 180 °F
Dry Time 2.00 - 4.00 hour
Moisture Content <= 0.20 %
Back Pressure 50.0 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Omni Plastics OmniLon™ PA6/6 GR33 HSH Nylon 6/6, 33% Glass reinforced
Omni Plastics OmniLon™ PA6 GR33 HS BCC12 Nylon 6, 33% Glass reinforced
Omni Plastics OmniLon™ PA6 GR13 Nylon 6, 13% Glass reinforced
Omni Plastics OmniLon™ PA6 GMR30 Nylon 6, 30% Glass/mineral reinforced
INEOS Styrolution Absolac® 100 ABS

POMNI5009 / 185155

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.