MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials Pearlstick™ 5714 F1 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Product Description: Pearlstick™ 5714 F1 is an aromatic polyether-based thermoplastic polyurethane; Main Applications: Solution coating

Availability: Africa & Middle East; Europe; Latin America; North America

Features: Aromatic

Uses: Coating Applications

RoSH Compliance: RoSH Compliant

Form: Pellets

Processing Method: Solution Coating

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 2781
Brookfield Viscosity 600 - 900 cP600 - 900 cPSpindle n°2, 20 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 80
@Time 1.00 sec
80
@Time 0.000278 hour
ISO 868
Tensile Stress 46.0 MPa6670 psiISO 527-2/5A/200
 4.00 MPa
@Strain 50 %
580 psi
@Strain 50 %
ISO 527-2/5A/200
 5.00 MPa
@Strain 100 %
725 psi
@Strain 100 %
ISO 527-2/5A/200
 10.0 MPa
@Strain 300 %
1450 psi
@Strain 300 %
ISO 527-2/5A/200
Elongation at Break 510 %510 %ISO 527-2/5A/200
Tear Strength 74.2 kN/m423 pliMethod Ba, Angle (Unnicked); ISO 34-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °FKofler

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUBRZ787 / 311480

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.