MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® Prism® 770 Primer
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes:
Surface Preparers
Loctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.

Loctite® Accelerators are used to increase the cure speed and gap filling capabilities of Cyanoacrylate Adhesives. Activators are specially engineered curing agents for Structural Adhesives. Loctite® Primers are used to ensure cure on inactive surfaces and speed the cure of machinery adhesives.

All Loctite® Surface Preparation products are available in ozone-safe (non-CFC) solvent-based and solventless formulations.

Loctite® 770 Heptane Base Prism® Primer
An adhesion promoter formulated for use with polyolefins and other low-energy surfaces. Use with Loctite® Cyanoacrylate Adhesives. Features fast dry time and long on-part life. Typical Use: All cyanoacrylates

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 1.25 cP
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 minDry Time
 8.00 hourOn-Part Life
 
Descriptive Properties
ColorColorless

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Tecothane® TT-2085A-B20 TPU – 20% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-2055D-B20 TPU – 20% Barium Sulfate
Lubrizol LifeSciences Tecothane® TT-1075D-M TPU - Clear
Lubrizol LifeSciences Tecothane® TT-1055D TPU - Clear
Henkel Loctite® 4981 Cyanoacrylate Adhesive

PLOCT145 / 51881

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.