MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Impact Grade

Material Notes: Description

LP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance.
Application

Applications of LP 551-01 include pails, housewares, heavy-duty crates, and industrial components. This resin meets FDA Regulation 21 CFR 177.1250, 3.1 and 3.2.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.953 g/ccASTM D792
ESCR 100% Igepal® 5.0 hourCondition B; ASTM D1693
Melt Index of Compound 7.0 g/10 minCondition E; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 59ASTM D2240
Tensile Strength, Yield 3200 psi2"/min; ASTM D638
Elongation at Break 100 %2"/min; ASTM D638
Flexural Modulus, 1% Secant 130000 psiASTM D790
Izod Impact, Notched 1.00 ft-lb/inASTM D256
Falling Dart Impact 24.0 ft-lb
@Temperature -40.0 °C
F50; ASTM D3029
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -92.0 °CASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Network Polymers NPP 50-0151
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
Network Polymers NPP 50-0350
Network Polymers NPP 50-0863
A. Schulman LP552-01 Injection Molding, Extrusion Grade Compound

PASHU085 / 25049

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.