MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Corr-Paint™ CP4010-S2-HT High Temperature Silicone Protective Coating  (discontinued **)
Categories: Polymer; Thermoset; Silicone

Material Notes: Aremco’s Corr-Paint™ CP40xx-S2 series silicone-ceramic coatings are single-part, room temperature cure systems that provide ultra-high temperature resistance up to 1800°F (982°C) along with exceptional resistance to outdoor weathering, UV, salt-spray corrosion, and flame impingement.

Product Highlights

  • Ultra-High Temperature Resistance
  • Room Temperature Curing
  • Single Part, No Catalyst Required
  • Sprayable, Low Viscosity
  • Moisture & Salt Spray Resistant
  • Flame Resistant
  • UV Resistant
  • High Dielectric Strength
Typical Applications
  • Ultra-High Temperature Resistance
  • Room Temperature Curing
  • Single Part, No Catalyst Required
  • Sprayable, Low Viscosity
  • Moisture & Salt Spray Resistant
  • Flame Resistant
  • UV Resistant
  • High Dielectric Strengtheners

Vendors: Aremco offers a broad range of coatings formulated using an advanced solvent-based silicone resin combined with inorganic fillers and pigments. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/cc
Solids Content 59.6 %59.6 %Volume
 67.3 %67.3 %Weight
Volatiles 32.4 %32.4 %
Viscosity 200 - 500 cP200 - 500 cP
Thickness 25.4 microns1.00 milDry Film Thickness
 42.7 microns1.68 milWet Film Thickness
Storage Temperature 4.44 - 32.2 °C40.0 - 90.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 593 °C1100 °FContinuous
 649 °C1200 °FIntermittent
Flash Point 42.2 °C108 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 4.44 - 32.2 °C40.0 - 90.0 °FApplication Temperature
Dry Time >= 1.00 hour>= 1.00 hourCuring, Min Air Set
 1.00 - 2.00 hour1.00 - 2.00 hourTouch
 2.00 - 4.00 hour2.00 - 4.00 hourHandling
 1.00 - 24.0 hour1.00 - 24.0 hourRecoat
Cure Time  60.0 min
@Temperature 232 °C
1.00 hour
@Temperature 450 °F
Option B
 1440 - 2880 min
@Temperature 22.8 °C
24.0 - 48.0 hour
@Temperature 73.0 °F
Option A
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorSilver
Theoretical Dry Film Coverage, ft2/gal955
ThinnerT-Butyl Acetate

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZPAREM967 / 316327

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.