MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond FDA12 Food and Drug Application Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND FDA12 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Administration, Chapter 1, Sub Part B, Sections 175.105 and 175.300. This two part light yellow adhesive is easily mixed, used and cured at room temperature for bonding, laminating and repair applications by manufacturers of food preparation, processing and packaging equipment, and by manufacturers of catheters, hearing aids, dental products and other biomedical instruments and devices. TRA-BOND FDA12 is an effective electrical insulator, and it provides low permeability to gases and vapors and good resistance to water, weather, galvanic action to petroleum solvents, lubricants and fuels, to mild acids and alkalis, and to many other organic and inorganic compounds. Though not fully cured, significant properties develop after 24 hours at 25°C.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccMixed
Solids Content 100 %Reactive Solids Content
Water Absorption 0.83 %After 24 hours
Viscosity 9000 cP
@Temperature 25.0 °C
Mixed (sp #4, 3 rpm)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82
Elongation at Yield 9.0 %
Adhesive Bond Strength 3500 psiLap shear, alum to alum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.20e+14 ohm-cm
Dielectric Constant 3.4
@Frequency 1000 Hz
Dielectric Strength 420 V/mil
Dissipation Factor 0.020
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 53.0 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 145 °C
Minimum Service Temperature, Air -70.0 °C
Glass Transition Temp, Tg 57.0 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 2.00 hour
@Temperature 65.0 °C
 72.0 hour
@Temperature 25.0 °C
Pot Life 50 min25 grams
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Color Light Yellow
Mix Ratio, parts by weight100/100Resin/Hardener
Thixotropic Index 13 rpm/30 rpm
Working Life hours 425 grams

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRAC255 / 71183

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.