Product Description: Forton 4184L6 DW is an easier flow version of Fortron 4184L4, for drinking water applications. This grade is especially used for thin walled parts requiring long flow lengths, stiffness and dimensional control. Applications made of this grade are typically electronic components. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Filler/Reinforcement: Glass Fiber/Mineral Additive: Flame Retardant; Mold Release; UV Stabilizer Features: Flame Retardant; Good Heat Resistance; UV Stabilized Uses: Automotive Applications Forms: Pellets Processing Method: Injection Molding Information provided by Celanese |