MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 1200 S-55D UV Ester-based Thermoplastic Polyurethane Elastomer, UV Stabilized
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D 792
Linear Mold Shrinkage 0.0090 cm/cm
@Thickness 3.17 mm
0.0090 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555instantaneous; ASTM D 2240
Tensile Strength at Break 49.0 MPa7100 psiASTM D 412
Tensile Stress at Strain  15.3 MPa
@Strain 50 %
2220 psi
@Strain 50 %
ASTM D 412
 16.2 MPa
@Strain 100 %
2350 psi
@Strain 100 %
ASTM D 412
 35.9 MPa
@Strain 300 %
5200 psi
@Strain 300 %
ASTM D 412
Elongation at Break 420 %420 %ASTM D 412
Flexural Modulus 0.172 GPa25.0 ksiASTM D 790
Tear Strength 175 kN/m1000 pliDie C; ASTM D 624
Compression Set 25 %
@Temperature 23.0 °C,
Time 79200 sec
25 %
@Temperature 73.4 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 221 °C400 - 430 °F
Mold Temperature 26.7 - 60.0 °C80.0 - 140 °F
Drying Temperature 107 °C225 °F
Dry Time 6 hour6 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 41.4 - 103 MPa6000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DSM Biomedical Bionate® 55D Thermoplastic Polycarbonate Polyurethane (PCU)
Huntsman IROGRAN® D 60 E 4024 Polyester-Based TPU-High Performance Grade
Taiwan Sheen Soon Sheenthane® D6010 Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer
DSM Biomedical Bionate® 90A Thermoplastic Polycarbonate Polyurethane (PCU)

PQZWA7418 / 92292

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.