MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Forged Plate  (discontinued **)
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Aluminum Alloy

Material Notes: Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent particle distribution and to enhance mechanical properties. Good machinability - use diamond tools and high feed/speed for best results.

Information provided by Aerospace Metal Composites Limited (AMC), acquired by Materion in 2012.

Key Words: Metal Matrix Composite - Silicon Carbide Particle Reinforced Aluminium; Al/SiC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.88 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 210Converted from Vickers
Hardness, Rockwell A 58.3Converted from Vickers
Hardness, Rockwell B 95Converted from Vickers
Hardness, Vickers 210Pryamidal Diamond 10 kg load
Tensile Strength, Ultimate 659 MPastatistical analysis gives AVG -3STD at 620 MPa
Tensile Strength, Yield 464 MPa
@Strain 0.2 %
statistical analysis gives AVG-3STD at 417 MPa
Elongation at Break 4.0 %in 50 mm
Tensile Modulus 115 GPa
Poissons Ratio 0.30
Fatigue Strength 210 MPa
@# of Cycles 100000
R=-1, Kt=1.75
 300 MPa
@# of Cycles 1.00e+7
RB R=-1
 430 MPa
@# of Cycles 100000
R=-1, Kt=1
Fracture Toughness 18.0 - 20.0 MPa-m½
Shear Modulus 44.0 GPaEstimated from similar metals.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000900 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.5 µm/m-°C
@Temperature -100 - 100 °C
Specific Heat Capacity 0.836 J/g-°C
Thermal Conductivity 150 W/m-K
@Temperature 0.000 - 100 °C
Melting Point 548 - 660 °C
Solidus 548 °C
Liquidus 660 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Extruded Bar
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition
Materion SupremEX® 640XA Aluminum - Silicon Carbide Metal Matrix Composite, T6 CWQ Billet
Materion SupremEX® 640XA Aluminum - Silicon Carbide Metal Matrix Composite, T7 Forged Plate
Ceramic Process Systems AlSiC-9, 63 vol% SiC

NAMC20 / 14952

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.