MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
NuSil EPM-2463 Silicone, Thermal Interface Material (TIM): Electrically Conductive
Categories: Polymer; Thermoset; Silicone

Material Notes: General Purpose: Thermal Interface Material (TIM): Electrically Conductive

Comments: Remains conductive over broad operating temperature range

Cure system: Tin/Oxime

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.30 g/cc
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Na (Sodium) <= 5.0 ppm
Ionic Impurities - K (Potassium) <= 10 ppm
Ionic Impurities - Cl (Chloride) <= 5.0 ppm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
Tensile Strength at Break 2.10 MPa
Elongation at Break 75 %
Tear Strength 55.0 pli
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.0020 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.50 W/m-KASTM C1045; ASTM E1530
 
Processing PropertiesOriginal ValueComments
Cure Time 168 hour
@Temperature 25.0 °C
Working Life 2.00 hour
@Temperature 25.0 °C
 
Descriptive Properties
ColorGreen-Gray
Mix Ratio100:0.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NuSil R-2634 Silicone, Electrically Conductive
Parker Chomerics CHO-SEAL 1221 Conductive Elastomer
P & P Technology EC-S Pure Silver Loaded Silicone
Parker Chomerics Tecknit Consil®-R 855 Pure Silver-Filled Silicone Elastomer
Parker Chomerics CHO-FORM 5531 EMI Shielding Material

PNUSIL262 / 141986

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.