MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron AboCoat 8709-7 Nickel-Filled Electrically Conductive Acrylic Compound
Categories: Polymer; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: AboCoat 8709-7 is an easy-to-use nickel-acrylic conductive coating.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 50.9 %
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 0.70 ohm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 80.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time >= 720 min
@Temperature 22.0 - 30.0 °C
 
Descriptive Properties
ColorGray
Metal (%)82.5of vehicle
ViscosityLow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asahi Kasei TENAC™-C TFC77 Copolymer Acetal (POM), Electrically Conductive
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic
Asahi Kasei Xyron™ X8610 PPE/PS, Electrically Conductive, High Stiffness, Carbon Fiber
Asahi Kasei TENAC™-C TFC64 Copolymer Acetal (POM), Electrically Conductive
Asahi Kasei TENAC™-C C84 Copolymer Acetal (POM), Electrically Conductive

PABC851 / 107835

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.