MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Astralloy Rol-Man® Steel Bolster Cup
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Patented Rol-Man® Flanged Bolster Cup is produced from 11% -14% manganese steel, AAR approved, and unique in simple design. Its innovative-flanged rim offers greater coverage and structural integrity where you need it most. No other combination of elements approaches the toughness, strength and wear resistance of Hadfield’s original manganese steel formula. Any steel that does not closely conform to the following chemical analysis is not true (11% - 14%) manganese steel. Rol-Man® rolled and forged manganese steel exactly follows this analysis. The Rol-Man® Flanged Bolster Cup is AAR approved under the provisions of S-3004. The approval process took several years of testing, tracking, and reporting of the cups’ superior in-service performance. Test cups in freight service have exceeded one million miles of satisfactory performance without replacement. Installation, maintenance or replacement is greatly simplified and extremely cost effective. No time consuming welding is required. The Rol-Man® Flanged Bolster Cup is tough, hard, and thrives on severe wear. It can be expected to last the life of the rail car. No lubrication is necessary with fully austenitic 11% to 14% manganese steel.

Information provided by Astralloy, a Nucor Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 180 - 220Hardness as Furnished
 500 - 650Work-Hardened
Hardness, Rockwell B 90 - 96
Hardness, Rockwell C 55 - 65
Tensile Strength 150 ksi
Tensile Strength, Yield 65.0 ksi
Elongation at Break 45 %
@Thickness 50.8 mm
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.0 - 1.4 %
Iron, Fe 84.3 - 87.9 %As Balance
Manganese, Mn 11 - 14 %
Phosphorus, P <= 0.016 %
Silicon, Si 0.10 - 0.30 %
Sulfur, S 0.010 - 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Grade 18Ni (250) Maraging Steel, 3.18 mm thick sheet, solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 480°C (900°F) for 3 hours
AISI Grade 18Ni (200) Maraging Steel, Annealed
216 Stainless Steel, Annealed Sheet, Strip (UNS S21600)
216 Stainless Steel, Annealed Plate (UNS S21600)
205 Austenitic Stainless Steel (UNS S20500)

NNUCOR922 / 233196

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.