MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
GEHR Plastics Noryl PPO-30 GF 30% Glass Filled
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 30% Glass Filled

Material Notes: PPO-30 GF is reinforced with 30% glass fiber for higher thermal properties and better dimensional stability. PPO belongs to the group of the amorphous materials and can be used in temperatures ranging from -58 °F to +302 °F. PPO exhibits a high impact strength and a very high dimensional stability. The electrical properties will not be influenced by the surrounding frequencies and therefore can be used in a lot of applications in electrical engineering.

Main Characteristics: high dimensional stability; low tendency to creep; high thermostability; high impact strength; good electrical characteristics over a far frequency range; high resistance to hydrolysis; self-extinguishing

Information provided by GEHR Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
Moisture Absorption at Equilibrium 0.060 %50% RH; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 89ASTM D2240
Tensile Strength at Break 17500 psiASTM D638
Elongation at Break 5.0 %ASTM D638
Modulus of Elasticity 1330 ksiASTM D638
Flexural Strength 25000 psiASTM D638
Izod Impact, Notched 2.20 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmASTM D257
Surface Resistance 1.00e+13 ohm
Dielectric Strength 20.9 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 µin/in-°FASTM D696
Maximum Service Temperature, Air 230 °FUL 746B
Deflection Temperature at 0.46 MPa (66 psi) 285 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 275 °FASTM D648
Vicat Softening Point 289 °FVST/B/50; ASTM D1525
Flammability, UL94 V-1UL 94
 
Compliance PropertiesOriginal ValueComments
FDA NoPhysiological indifference
 
Descriptive Properties
Acid ResistanceYes
Aromatic ResistanceNo
Bondabilityyes
CKW ResistanceNo
Hydrocarbonate ResistanceLimited
Hydroxide ResistanceYes
Ketone ResistanceNo
Physiological indifferenceno, NSF
Resistance to Hot WaterYes
UV Stabilizationlimited

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
GEHR Plastics Noryl PPO
Ensinger NORYL® Polyphenylene oxide (PPO)
Akro-Plastic Akrotek® PEEK CF 10 TM black (5050) PEEK, Dry, 10% Carbon Filled
Omnia Plastica Noryl® PPO m Polyphenylenoxide
Röchling SUSTAPEEK® GF 30 PEEK, 30% Glass Filled

PGEHR054 / 122037

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.