MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Quantum Composites QC-7810 55% Glass Fiber Polyester SMC  (discontinued **)
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: QC-7810 is a toughened thermoset polyester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength and flame resistance. It is suggested for applications subject to impacts and rough handling. QC-7810 has Underwriter's Laboratory recognition for 130°C use. Form and Color = Rolled Sheet, Black. Glass Fiber Length = .5 inch

A. Schulman has acquired Quantum Composites.

Key Words: Sheet Molding Compound
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.90 g/ccASTM D792
Water Absorption 0.10 %ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 68ASTM D2583
Tensile Strength, Ultimate 324 MPaASTM D638
Flexural Yield Strength 482 MPaASTM D790
Flexural Modulus 17.2 GPaASTM D790
Izod Impact, Notched 17.0 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °CUL Recognized
 >= 260 °CDeflection Temp; Load not reported; ASTM D648
Flammability, UL94 V-1
@Thickness 2.90 mm
Shrinkage 0.0010 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature 132 - 149 °CMold temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites QC-7753 50% Glass Fiber Reinforced Polyester SMC
IDI Composites 46-16-60 Thermoset Polyester, Sheet
IDI Composites A-207 Thermoset Polyester, Sheet
IDI Composites C-210 Thermoset Polyester, Sheet
Quantum Composites QC-8816 66% Glass Fiber Reinforced Polyester Hybrid SMC

PCOQC5 / 29042

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.