MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Barlog Plastics KEBAFLEX S FE 180401 natural SEBS
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: KEBAFLEX / S FE 180401 natural is a development product for the manufacture of flexible, flame-retardant components. KEBAFLEX / S FE 180401 natural has a Shore hardness of 80 A and, from a wall thickness of 1.6 mm, achieves the classification V0 based on the test standard UL 94. The material is suitable, among other things, for the manufacture of seals in electrical and electronic applications.

Properties: flexible, good haptics, good fire behavior, good recovery behavior, semi-crystalline, soft

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccISO 1183-1
Linear Mold Shrinkage, Flow 0.0200 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.00800 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80.0DIN ISO 7619-1
Tensile Strength at Break 3.80 MPaISO 527-1
Tensile Strength, Yield 1.50 MPa
@Strain 10.0 %
DIN EN ISO 527-1
Elongation at Break 200 %ISO 527-1
50% Modulus 2.50 MPa
@Strain 50.0 %
DIN EN ISO 527-1
100% Modulus 3.00 MPa
@Strain 100 %
DIN EN ISO 527-1
Tear Strength 12.0 kN/mDIN ISO 34-1
Compression Set 25.0 %
@Treatment Temp. 23.0 °C
ISO 815-1
 36.0 %
@Treatment Temp. 70.0 °C
ISO 815-1
 53.0 %
@Treatment Temp. 100 °C
ISO 815-1
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 0.400 mm
IEC 60695-11-10
 HB
@Thickness 0.800 mm
IEC 60695-11-10
 HB
@Thickness 1.60 mm
IEC 60695-11-10
 HB
@Thickness 3.20 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 190 - 220 °C
Mold Temperature 20.0 - 40.0 °C
Drying Temperature 80.0 °C
Dry Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBARLO544 / 326618

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.