MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastic Compounds Tehnamid® A-SV30-TAF Nylon 66, 30% Glass Fiber Reinforced, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: 30% glass-filled polyamide 66. Heat stabilized, anti-friction. Created for production by injection molding of various anti-friction products used in automotive, electronics and electrical engineering. Serially produced in natural color.

Information provided by Polyplastic Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³GOST 15139
Linear Mold Shrinkage, Flow 0.0015 - 0.0035 cm/cm0.0015 - 0.0035 in/inGOST 18616
Linear Mold Shrinkage, Transverse 0.0090 - 0.012 cm/cm0.0090 - 0.012 in/inGOST 18616
Melt Flow 10 - 20 g/10 min
@Load 2.16 kg,
Temperature 275 °C
10 - 20 g/10 min
@Load 4.76 lb,
Temperature 527 °F
GOST 11645
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 180 MPa26100 psiGOST 11262
Elongation at Break 3.0 %3.0 %GOST 11262
Flexural Strength 265 MPa38400 psiat maximum load; GOST 4648
Flexural Modulus 9.00 GPa1310 ksiGOST 9550
Charpy Impact Unnotched  5.50 J/cm²
@Temperature -40.0 °C
26.2 ft-lb/in²
@Temperature -40.0 °F
GOST 4647
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
GOST 4647
Charpy Impact, Notched  0.800 J/cm²
@Temperature -40.0 °C
3.81 ft-lb/in²
@Temperature -40.0 °F
GOST 4647
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
GOST 4647
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmGOST 6433.2
Dielectric Strength 28.0 kV/mm711 kV/inGOST 6433.3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C11.1 µin/in-°FGOST 15173
Melting Point 250 °C482 °FGOST 21553
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FGOST 12021
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °FGOST 12021

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLPLC130 / 307202

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.