MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECACOMP PK TRM PVX black 1015008 Polyketone, Carbon Fiber Reinforced, Graphite/PTFE Filled
Categories: Polymer; Thermoplastic; Polyketone

Material Notes:
  • good slide and wear properties
  • moderate stiffness
  • high toughness
  • hydrolysis resistant
  • high dimensional stability
  • low moisture absorption
  • resistant to many oils, greases and fuels
Target Industries:
  • automotive industry
  • mechanical engineering

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³
Water Absorption at Saturation 0.40 %0.40 %50 % relative humidity up to saturation; DIN EN ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inDIN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inDIN EN ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 90.0 MPa13100 psiDIN EN ISO 527-1
Elongation at Break 2.5 %2.5 %DIN EN ISO 527-1
Modulus of Elasticity 5.80 GPa841 ksiDIN EN ISO 527-1
Charpy Impact Unnotched 3.00 J/cm²14.3 ft-lb/in²DIN EN ISO 179-1eU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10000 ohm-cm10000 ohm-cmDIN EN 61340-2-3
Surface Resistance 10000 ohm10000 ohmDIN EN 61340-2-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F
Maximum Service Temperature, Air 100 °C212 °Flong term
 140 °C284 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 207 °C405 °FISO-R 75 Method A
Glass Transition Temp, Tg 12.0 °C53.6 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 220 - 265 °C428 - 509 °F
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIO9107 / 319035

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.