MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 Dynalife® HT NLGI Grade 2
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Dynalife HT is a high-quality, multipurpose, extreme-pressure (EP) lithium complex grease developed for the lubrication of automotive and industrial equipment operating under heavy loads and at moderate to high temperatures. It is recommended for use in a variety of automotive, agricultural, construction, mining and industrial applications. It is NLGI GC-LB certified for use as a multipurpose automotive wheel bearing and chassis lubricant. Dynalife HT is manufactured with high-quality base oils, a special polymer and a lithium complex soap thickener. It is fortified with extreme pressure and antiwear additives plus rust and oxidation inhibitors. It has excellent thermal stability at high temperatures, high load-carrying capacity for excellent wear protection, and protects metal parts against rust and corrosion. It forms an effective seal to help minimize bearing contamination. Its tackiness properties and heavy base oil provide a high level of adhesion to bearing surfaces for improved retention, reduced leakage and excellent resistance to water washout.

Applications:

  • Agricultural, construction, mining and industrial equipment operating under heavy or shock loads
  • Wheel bearings of passenger cars, trucks, high-performance vehicles, sport utility vehicles and motorcycles equipped with disc brakes
  • Ball joints, universal joints, other chassis parts and water pumps on passenger cars, trucks and other mobile equipment
  • Conveyor bearings
  • Pellet mills manufactured by Bliss Industries (Grade No. 2)
Features/Benefits:
  • Excellent high-temperature performance
  • Excellent wear protection
  • High load-carrying capacity
  • Protects against rust and corrosion
  • Excellent resistance to water washout
  • Good low-temperature pumpability
  • NLGI GC-LB certified

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.44 lb/gal
Viscosity Measurement 104Index
Saybolt Viscosity at 100°F 3350 SUS
Saybolt Viscosity at 210°F 195 SUS
Kinematic Viscosity at 40°C (104°F) 625 cSt
Kinematic Viscosity at 100°C (212°F) 40 cSt
Oxidative Stability 100 hour
@Pressure 0.0138 MPa
Pressure Drop; ASTM D942
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 315 kgASTM D2596
Four Ball Wear 0.450 mmScar Diameter; ASTM D2266
Penetration P(60), 1/10 mm 265 - 295ASTM D217
Timken Test 80.0 lbOK Load; ASTM D2509
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °C
Minimum Service Temperature, Air -12.0 °C
Dropping Point 260 °C
 
Descriptive Properties
ColorRed
ThickenerLithium Complex
Water Washout Resistance0.0275Weight Loss @ 175°F, ASTM D1264

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Polymist® F5A Polytetrafluoroethylene (PTFE) Powder
General Plastics LAST-A-FOAM® R-9320 Thermal Isolation Blocks
Dover Chemical EM 995 Fatty Amide Lubricity / Corrosion Inhibitor

WCON5113 / 198366

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.