MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos ABS Lustran® ABS 970  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Lustran® ABS 970 has high impact strength and good paintability.

Lustran® is now a product of INEOS Styrolution. Information provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cmISO 294-4
Melt Flow 22 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 108ISO 2039-2
Tensile Strength at Break 31.0 MPa50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 41.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break 20 %50 mm/min; acc. ISO 527-1,-2
Tensile Modulus 2.25 GPa1 mm/min; ISO 527-1,-2
Flexural Strength 67.0 MPa2 mm/min; ISO 178
Flexural Modulus 2200 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
 17.0 kJ/m²
@Temperature -20.0 °C
ISO 180-1A
 25.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °CISO 75-1,-2
Vicat Softening Point 98.0 °C
@Load 5.10 kg
120°C/hour; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 
Optical PropertiesOriginal ValueComments
Gloss 89 %Angle 60°; ISO 2813

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos ABS Lustran® ABS 680 LNS503 High Performance Injection Molding Grade
Ineos ABS Lustran® ABS 650 Injection Molding Grade
A. Schulman Diamond ABS 3500 HF Injection Molding Grade, High Flow, Medium Impact
Elix Polymers ELIX ABS P2M-AT Acrylonitrile Butadiene Styrene (ABS), High Impact Strength
Ineos ABS Lustran® 240 Injection Molding Grade

PINEA950 / 107221

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.