MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AK Steel 409 Ferritic Stainless steel
Categories: Metal; Ferrous Metal; Ferritic; Stainless Steel; T 400 Series Stainless Steel

Material Notes: AK Steel 409 Stainless Steels are especially useful for applications where oxidation or corrosion protection beyond the capacity of carbon steel and some coated steels is needed. Current applications include automotive and truck exhaust systems, including tubular manifolds; agricultural spreaders, gas turbine exhaust silencers, and heat exchangers. AK Steel 409 is also useful for "difficult-to-form" hardware such as fuel filters.

Information provided by AK Steel

Key Words: UNS S40920
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.61 g/cc0.275 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 66 - 72
@Thickness 1.02 - 1.78 mm
66 - 72
@Thickness 0.0400 - 0.0700 in
Annealed Condition
Tensile Strength, Ultimate 414 - 469 MPa
@Thickness 1.02 - 1.78 mm
60000 - 68000 psi
@Thickness 0.0400 - 0.0700 in
Annealed Condition
 6.20 MPa
@Thickness 1.14 - 1.52 mm,
Temperature 816 °C
899 psi
@Thickness 0.0449 - 0.0598 in,
Temperature 1500 °F
 10.3 MPa
@Thickness 1.14 - 1.52 mm,
Temperature 816 °C
1490 psi
@Thickness 0.0449 - 0.0598 in,
Temperature 1500 °F
 22.0 MPa
@Thickness 1.14 - 1.52 mm,
Temperature 704 °C
3190 psi
@Thickness 0.0449 - 0.0598 in,
Temperature 1300 °F
 27.5 MPa
@Thickness 1.14 - 1.52 mm,
Temperature 704 °C
3990 psi
@Thickness 0.0449 - 0.0598 in,
Temperature 1300 °F
Tensile Strength, Yield 241 - 283 MPa
@Strain 0.2 %,
Thickness 1.02 - 1.78 mm
35000 - 41000 psi
@Strain 0.2 %,
Thickness 0.0400 - 0.0700 in
Annealed Condition
Elongation at Break 31 - 39 %31 - 39 %in 2 inches, Annealed Condition (0.040" - 0.070")
Modulus of Elasticity 208 GPa30200 ksi
Fatigue Strength  10.0 MPa
@# of Cycles 1.00e+7 ,
Temperature 816 °C
1450 psi
@# of Cycles 1.00e+7 ,
Temperature 1500 °F
 117 MPa
@# of Cycles 1.00e+7 ,
Temperature 593 °C
17000 psi
@# of Cycles 1.00e+7 ,
Temperature 1100 °F
 324 MPa
@# of Cycles 1.00e+7
47000 psi
@# of Cycles 1.00e+7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000600 ohm-cm0.0000600 ohm-cm
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.020 %<= 0.020 %
Chromium, Cr 10.5 - 11.7 %10.5 - 11.7 %
Iron, Fe >= 85.3 %>= 85.3 %As Remainder
Manganese, Mn <= 0.75 %<= 0.75 %
Nickel, Ni <= 0.50 %<= 0.50 %
Nitrogen, N <= 0.020 %<= 0.020 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.020 %<= 0.020 %
Titanium, Ti 0.15 - 0.50 %0.15 - 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
409 Stainless Steel
304 Stainless Steel
316 Stainless Steel, annealed sheet
409 Stainless Steel, annealed sheet, strip, plate, bar
Type 439 Ferritic Stainless Steel, Annealed Bar, UNS S43035

NAKS093 / 14696

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.