MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake EMAC® Plus SP1305 20% Ethylene-Methyl Acrylate Copolymer
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate

Material Notes: Westlake EMAC® Plus SP1305 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1305 is compatible with and provides excellent adhesion to polyolefins, polyesters, and other polymers while providing outstanding low temperature performance. The higher melting point of this EMAC® Plus grade offers EMA performance with improved heat resistance.

Applications: films, disposable gloves, and wound care.

FDA: This material complies with FDA regulations in 21 CFR, section 177.1340.

All information provided by Westlake Chemical

Key Words: Excellent adhesion to polyolefins, polyesters, and other polymers while providing outstanding low temperature performance
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.942 g/ccASTM D1505
Methyl Acrylate Content 20 %
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 37ASTM D2240
Tensile Strength at Break 11.0 MPa500mm/min; ASTM D638 Type IV Specimen
Elongation at Break 815 %500mm/min; ASTM D638 Type IV Specimen
 
Thermal PropertiesOriginal ValueComments
Melting Point 96.0 °Cby DSC; ASTM D3418
Vicat Softening Point 50.0 °CASTM D1525
Brittleness Temperature <= -73.0 °CASTM D746
 
Descriptive Properties
ProcessBlown Film
 Extrusion
 Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake EMAC® SP2220 20% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2207 20% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2205 20% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2202 21.5% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SA2413 Ethylene Methyl Acrylate Copolymer

PWESF001 / 84438

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.