MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parson Adhesives SONLOCK™ 3542 Anaerobic Thread Sealant
Categories: Polymer; Adhesive; Thermoset

Material Notes: SONLOK 3542 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures rapidly in the absence of air between close fitting metal surfaces and provide low-pressure resistance immediately after application. SONLOK 3542 is ideal to seal against gases, water, LPG, hydrocarbons, oils and other chemicals. Excellent thixotropic property prevents migration of the sealant before or during curing.

Applications:

  • Ideal for locking and sealing of threaded metal pipes and fittings
  • Low viscosity with medium strength sealing properties.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/cc
Brookfield Viscosity 525 - 1850 cP525 - 1850 cPThixotropic, RVT, Spindle 3 @ 20 rpm
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 6.48 MPa940 psiSteel Pins & Collars; ISO 10123
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FASTM D696 K-1
Specific Heat Capacity 0.300 J/g-°C0.0717 BTU/lb-°F
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
Flash Point >= 100 °C>= 212 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 - 30.0 min0.167 - 0.500 hourHandling
 120 - 240 min2.00 - 4.00 hourFunctional
 1440 min24.0 hourFull
 
Descriptive Properties
ColorBrown
CompositionMethacrylate Ester
Initial Strength Retained (%)100Motor Oil for 500 hrs at 125°C
 100Motor Oil for 1000 hrs at 125°C
 100Gasoline for 500 hrs at 22°C
 100Ethanol for 500 hrs at 22°C
 100Break Fluid for 500 hrs at 22°C
 80Acetone for 500 hrs at 22°C
 80Acetone for 1000 hrs at 22°C
 90Water/Glycol for 500 hrs at 87°C
 90Water/Glycol for 1000 hrs at 87°C
 95Break Fluid for 1000 hrs at 22°C
 95Ethanol for 1000 hrs at 22°C
 95Gasoline for 1000 hrs at 22°C
Solvent ContentNone
Torque15 NmBreakaway, M10 steel nuts and bolts, ISO 10964
 25 NmBreakloose, Pre-torqued to 5 Nm, M10 steel nuts and bolts, ISO 10964
 25 NmMax Prevail, Pre-torqued to 5 Nm, M10 steel nuts and bolts, ISO 10964
 9 NmPrevail, M10 steel nuts and bolts, ISO 10964

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPARSN036 / 186479

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.