MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Eastman Diphenyl oxide Process Fluid
Categories: Fluid

Material Notes: CAS No. 101-84- 8

Product Description: Applications for diphenyl oxide process fluid include process media, raw materials, or solvents in many industries, including chemicals, fragrances, and petrochemicals.

Application/Uses:

  • High boiling point
  • High flash point
  • High purity (>99.9%)
  • High solvency
  • High thermal stability
  • Low polarity
  • Low reactivity
  • Noticeable odor

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/cc
Viscosity Measure 2.58 cSt
@Temperature 38.0 °C
Kinematic
Molecular Weight 170 g/mol
Vapor Pressure 0.0000600 atm
@Temperature 93.0 °C
 
Thermal PropertiesOriginal ValueComments
Boiling Point 258 °C
Flash Point 115 °CASTM D92
 
Descriptive Properties
AppearanceClear colorless liquidAbove 69°C
 White solidBelow 69°C
Content<100Bromine index, ASTM D2710
 <150 ppmMoisture
Fire Point125°CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5103 / 222297

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.