MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem ZINC OXIDE USP-2
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Zinc Oxide USP-2 is produced from the highest quality and purity zinc metal under carefully controlled conditions. It is specially produced to comply with the high purity requirements of the United States Pharmacopeia and the FDA (21 CFR 73.1991). USP-2 provides excellent physical properties, has a bright blue-white color, fine texture and optimum particle size for maximum dispersion.

Uses: Zinc Oxide USP-2 is used in applications requiring high purity zinc oxide. Applications that include compliance with FDA, dental, cosmetic and pharmaceutical standards and is prescribed in The National Formulary.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 5.61 g/cc
Particle Size 0.33 µmMean
Particle Mesh Size 325 Mesh99.99% passing
Specific Surface Area 3.2 m²/g
 
Component Elements PropertiesOriginal ValueComments
CdO 0.0010 %
SO3 0.0010 %
 
Descriptive Properties
Absorption12 gms/100gms
Content<0.00003%As2O3
 <0.01%Insoluble in HCL
 0.0002H2O Soluble Salts
 0.0004Loss @ 110oC
 0.999ZnO (Dry Basis)
 1E-05PbO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH654 / 315572

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.