Hostacom 1202 1053 is a 20% talc filled polypropylene copolymer, with high melt flow rate, good impact/stiffness balance, and good UV resistance. Product is available as a customized color matched, pellet form. This grade is delivered in 1053 color version. Applications: AppliancesInformation provided by LyondellBasell. |