MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chengdu Polyster MCA Melamine Cyanurate
Categories: Polymer; Thermoset; Melamine

Material Notes: White crystal power with satiny. It is an excellent non-halogen N flame retardant. The product is mainly used as non-halogen flame retardant for synthetic resin(PA, PVC, PS, POM), synthetic rubber and plastic products; solid lubricant in lubricating oil and grease; fire retardant in fire-proofing coating; lubricant in lubricating oil and grease; fire retardant in fire-proofing coating; lubricant in the cosmetic. MCA is used specifically for PA6 and PA66 without packing.

Information provided by Chengdu Polyster Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.450 - 0.550 g/cc
Density 1.50 - 1.60 g/cc
Solubility in Water 0.0010 %
pH 5.0 - 7.0
 
Thermal PropertiesOriginal ValueComments
Sublimation Temperature 440 °C
Flammability, UL94 V-0
@Thickness 1.60 mm
 
Descriptive Properties
Cyanuric Acid Content (%)0.2
Dry Weightless (%)0.2
Melamine Content (%)0.1
Melamine Cyanurate (%)99.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Perstorp Compounds Aminel FX Melamine
Oceanchem Group Melamine Cyanurate (MCA)
Overview of materials for Urea Formaldehyde, Molded, Cellulose Filled
Raschig Group MELOPAS® 156 MF Melamine
Raschig Group MELOPAS® 2010 MF Melamine

PCHEN020 / 79317

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.