General purpose steel with good corrosion resistance. Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets. Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms. |
EN 1.4306; ASTM 304L; JIS SUS 304L |