MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cyclohexene (C6H10)
Categories: Fluid; Solvent

Key Words: C6H10
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.8102 g/cc
@Temperature 20.0 °C
0.02927 lb/in³
@Temperature 68.0 °F
Viscosity  0.625 cP
@Temperature 25.0 °C
0.625 cP
@Temperature 77.0 °F
 0.65 cP
@Temperature 20.0 °C
0.65 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 82.15 g/mol82.15 g/mol
Vapor Pressure  0.093848 bar
@Temperature 20.0 °C
70.392 torr
@Temperature 68.0 °F
 0.1000 bar
@Temperature 21.0 °C
75.00 torr
@Temperature 69.8 °F
Extrapolated beyond actual measurements.
Surface Tension 26.17 dynes/cm
@Temperature 25.0 °C
26.17 dynes/cm
@Temperature 77.0 °F
Gamma
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 43.5 bar32600 torr
Critical Temperature 287.28 °C549.10 °F
Critical Density 0.281 g/cc0.0102 lb/in³
Critical Molar Volume 292 cm³/mol17.8 in³/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.222.22
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 40.05 J/g17.23 BTU/lbEnthalpy of fusion at normal melting point
Heat of Vaporization 370.8 J/g159.5 BTU/lbEnthalpy of vaporization at normal boiling temperature
Specific Heat Capacity 1.263 J/g-°C
@Temperature 25.0 °C
0.3019 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.130 W/m-K
@Temperature 25.0 °C
0.902 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
Melting Point -103.5 °C-154.3 °FAt atmospheric pressure (760 torr)
Boiling Point 83.0 °C
@Pressure 0.101 MPa
181 °F
@Pressure 14.7 psi
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4465
@Temperature 20.0 °C,
Wavelength 589.3 nm
1.4465
@Temperature 68.0 °F,
Wavelength 589.3 nm
Na D line
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter15.8243
Antoine's Vapor Pressure B Parameter2813.53
Antoine's Vapor Pressure C Parameter-49.98
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)110-83-8
Chemical FormulaC6H10
Critical Compressibility (Zc)0.27
Dipole moment (p/C.m)2.001E-28
Molar Heat Capacity (298K)103.719 J/mol-K
Molar Heat Capacity of Vapor a Parameter-68.605
Molar Heat Capacity of Vapor b Parameter0.7247
Molar Heat Capacity of Vapor c Parameter-0.000541
Molar Heat Capacity of Vapor d Parameter1.643E-07
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1146

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
2-Octanol, C8H18O
2-Butoxyethanol, C6H14O2
2-Butanol (CH3CH2CH(OH)CH3; secondary-Butyl Alcohol)
1-Pentanol, C5H12O
1-Octanol, C8H18O

VORG011 / 74522

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.