MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lubrizol Advanced Materials Stat-Rite® SIS-534 High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Product Description: SIS-534 sheet utilizes Lubrizol’s patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to enhance standard HIPS packaging sheet with a layer of clean, permanent ESD protection. It provides more consistent ESD protection than coatings or anti-stat. The Stat-Rite® skin will NOT deteriorate or wash off over time, thus providing reliable ESD protection for many years. Features: More permanent than anti-stat; Provides protection for many years; Good rigidity; Cleaner and more consistent that anti-stats or coatings; Colorable. Applications: Electronic assembly packaging; Electronic component packaging
Availability: Asia Pacific, Europe, Latin America, North America
Features: Antistatic; Clean/High Purity; Durable; ESD Protection; Good Colorability; Medium Rigidity; Rapid Static Decay; Wear Resistant
Uses: Electrical/Electronic Applications
Appearance: Violet
Forms: Sheet

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.7 MPa3000 psiASTM D638
Elongation at Break 85 %85 %ASTM D638
Tensile Modulus 1.38 GPa200 ksiASTM D638
Flexural Modulus 1.38 GPa200 ksiASTM D790
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 2.00e+9 ohm2.00e+9 ohm12% RH; ESD S11.11
Surface Resistivity per Square 5.00e+9 ohm5.00e+9 ohm50% RH; ASTM D257
Static Decay 0.020 sec0.020 sec-5000 V to -50 V, FTMS-101C, 12% RH
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUBR6026 / 268328

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.