MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LG Chemical NBR 2255 High Acrylonitrile Polymer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: NBR 2255 is a copolymer of butadiene and acrylonitrile to be manufactured by cold emulsion polymerization through the advanced technology and process of LG Chem. NBR 2255 is a non staining, medium Mooney, and low acrylonitrile polymer designed to aid in processing operations such as extrusion and press molding. And also, this grade offers excellent flexibility and elasticity in low temperature by the minimized block structure and low acrylonitrile content on polymer chain. NBR 2255 is preferably used for industrial belt, hoses, and many rubber parts such as seal and gasket. And also, it can be used for the industrial roller and low hardness roller of office printer due to good dynamic elasticity.

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³
Volatiles 0.20 %0.20 %
Mooney Viscosity 55
@Temperature 100 °C
55
@Temperature 212 °F
ML1+4
Ash 0.40 %0.40 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 26.0 MPa3770 psi145°C×50min. Cured; ASTM D412
Elongation at Break 465 %465 %145°C×50min. Cured; ASTM D412
300% Modulus 15.2 MPa
@Strain 300 %
2200 psi
@Strain 300 %
145°C×50min. Cured; ASTM D412
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month
@Temperature <=30.0 °C
18.0 Month
@Temperature <=86.0 °F
 
Descriptive Properties
Bound AN Content (%)22
ColorLight Tan
StabilizerNon-Staining

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Nitriflex NitriClean 2858 NBR - Nitrile Rubber
Nitriflex N-612B NBR - Nitrile Rubber
LG Chemical NBR 6230 High Acrylonitrile Polymer

PLHCHEM9849 / 239365

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.