MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP PP 30 GF FR0 NAT Polypropylene (PP), Glass Fiber - Flame Retardant - Value Product - UL94
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Flame Retardant - Glass Fiber - Value Product

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.46 g/ccASTM D 792
Additive Loading 30 %Primary Additive
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
@Thickness 3.17 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 105ASTM D 785
Tensile Strength at Break 10000 psiASTM D 638
Elongation at Break 2.0 - 4.0 %ASTM D 638
Tensile Modulus 1100 ksiASTM D 638
Flexural Strength 16000 psiASTM D 790
Flexural Modulus 900 ksiASTM D 790
Izod Impact, Notched 1.80 ft-lb/in
@Thickness 3.17 mm
ASTM D 256
Izod Impact, Unnotched 10.0 ft-lb/in
@Thickness 3.17 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D 257
Dielectric Constant 3.3
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dielectric Strength 450 V/milshort term, in oil; ASTM D 149
Dissipation Factor 0.0030
@Frequency 1e+6 Hz
Dry; ASTM D 150
Arc Resistance 85 secASTM D 495
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 310 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 290 °FASTM D 648
Flammability, UL94 V-0
@Thickness 0.7937 mm
 V-0
@Thickness 3.17 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 375 - 450 °F
Mold Temperature 90.0 - 150 °F
Drying Temperature 175 °F
@Time 7200 sec
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP PP 30 GF BLK Polypropylene (PP), Value Product - Glass Fiber - Chemically Coupled
RTP Company RTP PP 30 GF NAT Polypropylene (PP), Value Product - Glass Fiber - Chemically Coupled
Celanese Coolpoly® D1202 Thermally Conductive Polypropylene
GEHR Plastics PP-30GF Polypropylene, 30% Glass Fiber
RTP Company RTP PP 30 GF FR0 BLK Polypropylene (PP), Glass Fiber - Flame Retardant - Value Product - UL94

PQZTA5675 / 159106

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.