MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SunChemical Gwent R2040227D1 Hot Melt Conductive Adhesive for Diagnostic Sensors
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: This is a one-component water based polyurethane dispersion used for bonding unsupported PVC foils. This can be used in many different diagnostic applications such as test cards, assays and support systems for membrane-based immunodiagnostic tests.

The paste is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 43 - 47 %
Viscosity 1700 - 1900 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
Haake VT 550 PK1.1°
Storage Temperature >= 5.00 °Ccool dry place
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 °C
 70.0 - 80.0 °Cactivation temperature used to laminate with a press or vacuum tube
Cure Time 0.25 - 0.5 hour
Shelf Life 6.00 Month
 
Descriptive Properties
Coverage m2/ltr12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem Evateno® HM 150 EVA Hot Melt Copolymer
Kuraray SEPTON® A2 Hot Melt Adhesive
Master Bond MB529 Acrylic Polymer Based, Hot Melt Adhesive System
Wanhua Chemical Wanthane® WHT-6275 TPU Hot-Melt Adhesive
3M Scotch-Weld™ 3731 Hot Melt Adhesive

WGEM045 / 75898

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.