MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Clyrell EC 340Q Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: The specialty polypropylene Clyrell product portfolio includes random and impact copolymers based on Ziegler-Natta catalysts. Clyrell EC340Q is a specially designed nucleated polypropylene impact copolymer for injection molding. Clyrell EC340Q offers an excellent impact strength/stiffness combination, easy processing, low stress whitening with very high gloss and low shrinkage for its use in toys, sport, leisure, food packaging, containers, house wares, consumer goods and similar applications.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 22 g/10 min
@Load 2.16 kg,
Temperature 230 °C
22 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 23.0 MPa3340 psiISO 527-1,-2
Elongation at Break >= 50 %>= 50 %ISO 527-1,-2
Elongation at Yield 13 %13 %ISO 527-1,-2
Tensile Modulus 1.15 GPa167 ksiISO 527-1,-2
Charpy Impact, Notched  0.400 J/cm²
@Temperature -20.0 °C
1.90 ft-lb/in²
@Temperature -4.00 °F
Type 1, Edgewise, Notch A; ISO 179
 0.550 J/cm²
@Temperature 0.000 °C
2.62 ft-lb/in²
@Temperature 32.0 °F
Type 1, Edgewise, Notch A; ISO 179
 2.20 J/cm²
@Temperature 23.0 °C
10.5 ft-lb/in²
@Temperature 73.4 °F
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C190 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 127 °C261 °FA50; ISO 306
Brittleness Temperature -46.0 °C-50.8 °FISO 6603-2
 
Optical PropertiesMetricEnglishComments
Haze 38 %
@Thickness 1.00 mm
38 %
@Thickness 0.0394 in
ASTM D1003
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQT7095 / 218732

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.