MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Henkel Loctite® 3151 1 component acrylic UV/Heat Cure Acrylic Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes:
Thermally Conductive Bonders
Loctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or microprocessors and their heat sinks. Loctite offers a wide range of adhesive chemistries including silicones, acrylics and epoxies. Many processing options are available for curing these adhesives such as heat cure, activator cure, and UV light.

Loctite® 3151 1 component acrylic UV/Heat Cure Acrylic Adhesive
A self-shimming, UV and heat cure repairable adhesive for automated heat sink applications. Cure Type: UV/Heat

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.70 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 400000 psi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.810 W/m-K
Glass Transition Temp, Tg 50.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.170 minFixture time @ 70 - 100 mW/cm^2
 300 secFull Cure Time @ 150-180ºC
Shelf Life 9.00 Monthshelf life at 5ºC
 
Descriptive Properties
ViscosityPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Loctite® Output™ 383 Acrylic Adhesive
Henkel Loctite® Output™ 315 Acrylic Adhesive
Henkel Loctite® Output™ 384 Thermally Conductive Repairable Acrylic Adhesive
3M 760 Hybrid Adhesive Sealant
Aptek UVIBOND 7100 Semi-rigid, UV-Curing Urethane Adhesive

PLOCT168 / 51904

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.