MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt STYPOL® 040-4950 Marble Clear Gel Coat
Categories: Polymer; Thermoset

Material Notes: STYPOL® 040-4950, 040-4954, 040-4956 and 040-4965 are clear MACT compliant NPG isophthalic gel coats. They have been designed for use in the manufacturing of cultured marble, onyx, and granite.

Features and Benefits:

  • Low VOC / HAP content (42% or less)
  • Excellent sprayability
  • Excellent nonsagging properties
  • High clarity
  • Excellent chemical and water resistance
  • Excellent thermal shock resistance
  • UV light stabilized
  • Good color retention
  • Suitable for low pressure spray equipment
  • Meets gel coat test specifications according to ANSI Z124.3
  • Meets BAAQMD, Regulation 8-50-1, Method 26 (Bay Area AQMD of Northern California)

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.089 g/cc0.03934 lb/in³
Volatile Organic Compounds (VOC) Content 42 g/l42 g/l
Brookfield Viscosity 3000 cP3000 cPRVF #3 Spindle, 20 rpm @ 77°F
 
Processing PropertiesMetricEnglishComments
Cure Time 35.0 min
@Temperature 25.0 °C
0.583 hour
@Temperature 77.0 °F
Castable Time, 2% Arkema DDM-9 @ 77°F
Gel Time 6.00 min
@Temperature 25.0 °C
6.00 min
@Temperature 77.0 °F
2% Arkema DDM-9 @ 77°
 
Descriptive Properties
Thixotropic Index6.42/20 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9269 / 231864

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.