Borcycle™ EE0300SY is a 6 % mineral filled polypropylene compound containing 30% post-consumer recycled polymer and is intended for injection molding. This material has an excellent balance between impact strength and stiffness and gives a good surface quality. Special Features: - Excellent scratch resistance
- Low density
- Good surface aesthetics
- Low volatiles
Applications: Borcycle EE0300SY has been developed especially for the car industry to be used in automotive interior parts. - Door panels and pockets
- Interior trims
- Pillar trims
- Tailgate claddings
Values determined on standard injection molded specimens conditioned at 23°C and 50% relative humidity after at least 96 hours storage time. To avoid residual humidity from transport or storage, the material should be pre-dried approximately 2h at 80°C.Information provided by Borealis AG |