MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Chemlon® 60GS8H Nylon 6, 40% Glass Sphere Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Bead Filled

Material Notes: Notes: 60GS8H is a 40% glass sphere filled, heat stabilized of nylon 6 that offers excellent rigidity coupled with minimal distortion.

Availability: Europe; North America

Fillers/Reinforcement: Glass Bead, 40% Filler by Weight

Additive: Heat Stabilizer

Features: Heat Stabilized; High Rigidity

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.0 %1.0 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0060 - 0.015 cm/cm0.0060 - 0.015 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 88.3 MPa12800 psiISO 527-2
Elongation at Break 4.0 %4.0 %ISO 527-2
Tensile Modulus 4.80 GPa696 ksiISO 527-2
Flexural Strength 125 MPa18100 psiISO 178
Flexural Modulus 2.45 GPa356 ksiISO 178
Charpy Impact Unnotched 3.15 J/cm²15.0 ft-lb/in²ISO 179
Charpy Impact, Notched 0.609 J/cm²2.90 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant 3.83.8IEC 60250
Dielectric Strength 9.84 kV/mm
@Thickness 3.00 mm
250 kV/in
@Thickness 0.118 in
IEC 60243-1
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 525 V525 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) >= 200 °C>= 392 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FUnannealed; ISO 75-2/A
Oxygen Index 22 %22 %ISO 4589-2
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 240 - 290 °C464 - 554 °F
Middle Barrel Temperature 240 - 290 °C464 - 554 °F
Front Barrel Temperature 240 - 290 °C464 - 554 °F
Melt Temperature <= 300 °C<= 572 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour
Screw Speed 50 - 200 rpm50 - 200 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0389 / 236880

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.