MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Superior Flux Superior No. 325 Alcohol-Based, No-Clear Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Eliminates the need for cleaning soldered boards.
  • Increased activity level.
  • Can be used with lead free solder.
  • Excellent for wire tinning in automated and manual wire tinning systems.
  • A good flux for hand soldering PCB assemblies in touch-up or build-out processes.
  • Low solids content.
Description: Superior No. 325 flux is formulated for spray fluxing application in wave soldering. It can also be used for wire tinning applications. Superior No. 325 is an alcohol-based No-Clean flux that contains non-halide activators. The absence of halides and the very low solids content of the flux leaves parts with only negligible traces of low reactivity residues. The flux contains virtually no water and will not spatter on contact with molten solder. This flux contains no rosin or resins, and successfully replaces rosin fluxes.

Applications: WAVE SOLDERING-Superior No. 325 may be applied by foam, spray, or wave application. The topside board preheat temperature recommendation is 93-115°C/200-240°F.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.795 - 0.815 g/cc0.795 - 0.815 g/cc
Density 0.830 g/cc0.0300 lb/in³
Solids Content <= 3.5 %<= 3.5 %
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 25 - 3025 - 30
 
Thermal PropertiesMetricEnglishComments
Boiling Point 78.3 °C173 °F
Flash Point 15.5 °C59.9 °FTCC Method
 
Processing PropertiesMetricEnglishComments
Processing Temperature 390 - 500 °C734 - 932 °FSoldering Range
Shelf Life 2.00 Month2.00 Month
 
Descriptive Properties
FormClear Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Touchstone CFOAM® 17 Structural Carbon Foam
Thermal Ceramics Cease 2000 Fire
Pyrotek Mesh core / Z-6W Tadpoles
Pyrotek Mesh core / V-5 Tadpoles
Pyrotek Jacketed mesh core Tadpoles

NSFLUX053 / 185737

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.