MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Indium Corp. Indalloy® 227 Sn-In-Ag Solder Alloy
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy; Tin Alloy

Material Notes: Pb free solder can be used as a replacement for 63Sn 37Pb, 62Sn 36Pb 2Ag and 60Sn 40Pb in that it has similar physical and mechanical properties. Not for use over 100°C due to 118°C Sn/In eutectic.

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.25 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 17
Tensile Strength, Ultimate 46.9 MPa
Elongation at Break 47 %
Modulus of Elasticity 5600 ksi
Shear Strength 33.1 MPaShear Bond Holding Strength
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000180 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 28.0 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 54.0 W/m-K
@Temperature 85.0 °C
Melting Point 175 - 187 °C
Solidus 175 °C
Liquidus 187 °C
 
Component Elements PropertiesOriginal ValueComments
Indium, In 20 %
Silver, Ag 2.8 %
Tin, Sn 77.2 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Indium Corp. Indalloy® 231 Sn-Zn-In-Bi Solder Alloy
Indium Corp. Indalloy® 254 86.9Sn/10.0In/3.1Ag Lead-Free Solder Alloy
Indium Corp. Indalloy® 121 Sn-Ag Solder Alloy
Indium Corp. Indalloy® 133 Sn-Sb Solder Alloy
Indium Corp. Indalloy® 209 Sn-Ag-Sb Solder Alloy

NNIN26 / 18482

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.