Sequel 1714-1 FP BLK thermoplastic polyolefin material is typically used for painted automotive exterior applications. This material exhibits excellent durability and ductile low-temperature impact properties. Applications: Automotive Parts, Bumpers, Exterior Automotive ApplicationsInformation provided by LyondellBasell. |