MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Synthos SYNTECA® 63/63G Polybutadiene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: SYNTECA® NdBR and NiBR are used in the tire industry for tread and sidewall compounds, and in other industries for a range of elastomeric products such as conveyor belts and golf balls. Due to its low glass transition temperature, low dispersity level and linear structure, SYNTECA® NdBR is particularly suitable for tread compounds for the development of ‘green tires’, as it offers excellent wear properties and enables a reduction in fuel and energy consumption due to its very low rolling resistance.

Information provided by Synthos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 0.15 - 0.80 %0.15 - 0.80 %63G
 0.50 %0.50 %63
Mooney Viscosity 63
@Temperature 100 °C
63
@Temperature 212 °F
ML(1+4), unmassed
Ash 0.20 - 0.70 %0.20 - 0.70 %
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -108 °C-162 °F
 
Descriptive Properties
CatalystNd
Content98, > 96%Cis structures

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSYNTHOS015 / 320296

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.