MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

STAR Thermoplastic Alloys & Rubbers StarBond™ 4052 OM-B TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Features: Soft-touch TPEs for overmolding applications; Rubbery feel; Wide range of hardness; Improved haptics; Excellent adhesion to polar substrates such as polycarbonate, SAN, ASA, ABS, Polyester and Polyamide

Benefits: Design flexibility; Colorabilty; Overall feel; Visual appeal; Adhesion to polar substrates; Requires no drying; UV Resistant

Application Examples: Toothbrush grips; Razor grips; Smart device accessories; Tool grip handles; Game consoles; Caster wheels; Utensil handles

Information provided by Star Thermoplastic Alloys & Rubbers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.950 g/cc0.950 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5353
Tensile Strength 6.950 MPa1008 psi
Elongation at Break 702 %702 %
300% Modulus 3.34 MPa485 psi
Tear Strength 75.7 kN/m432 pli
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTAQ7047 / 307272

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.