MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Reliance Industries Repol R110MK Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: REPOL Polypropylene R110MK is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol R110MK is recommended for use in injection molding processes. It is an ideal material for attaining high clarity in houseware and industrial products. This grade is recommended for non food contact applications. Repol R110MK contains clarifier and antistatic agent that reduces static charge buildup on products.

Features:

  • Consistent processability
  • Good clarity
  • Superior mechanical properties
  • Low static charge build-up and reduced dust pickup
  • Information provided by Reliance Industries

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Melt Flow 12 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    12 g/10 min
    @Load 4.76 lb,
    Temperature 446 °F
    ASTM D1238
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength, Yield 28.0 MPa4060 psi50mm/min; ASTM D638
    Elongation at Yield 12 %12 %50mm/min; ASTM D638
    Flexural Modulus, 1% Secant 1300 MPa189000 psiASTM D790A
    Izod Impact, Notched 0.600 J/cm
    @Temperature 23.0 °C
    1.12 ft-lb/in
    @Temperature 73.4 °F
    ASTM D256
     
    Thermal PropertiesMetricEnglishComments
    Melting Point 150 °C302 °FDSC second heating; ASTM D3418
    Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FASTM D648

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Pinnacle Polymers 3220 Impact Polypropylene Copolymer, Injection Molding Grade
    Pinnacle Polymers 5112 C Clarified Random Polypropylene Copolymer, Injection Molding Grade
    Pinnacle Polymers 1335 Z Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat
    Pinnacle Polymers 2135 Impact Polypropylene Copolymer, Injection Molding Grade
    Pinnacle Polymers 3208 High Impact Polypropylene Copolymer, Injection Molding Grade

    PREL049 / 65389

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.