Product Description: A biaxially oriented polypropylene film metallizable on one side, with a heat sealable surface on the other side. Designed to be used after metallization as a single web in HFFS applications or in laminations for other purposes. Availability: Africa & Middle East, Asia Pacific and Europe Key Features: - Good adhesion layer for metallization
- Excellent processability in metallization
- Good machinability on HFFS machine
- Very good hot tack
- One side sealable
- High yield
- Brilliant metal appearance after metallization
Features:- In Lamination Lap Sealable
Applications: Uses: - HFFS Flexible PackagingInformation provided by ExxonMobil
|