MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Metton LMR M2100VO Liquid Molding Resin
Categories: Polymer; Thermoset; Polydicyclopentadiene (PDCPD)

Material Notes: Metton LMR is a tough and durable engineering plastic material used to produce large or thick molded parts for many diversified applications. The Metton LMR reaction injection molding process can provide large parts in low pressure molds with the mechanical property performance similar to injection molded engineering thermoplastics. The combination of Metton LMR’s process and material capabilities result in a new design freedom for replacing traditional materials such as metal, wood and fiberglass.

Injection molded engineering thermoplastics have a similar benefit package for smaller parts. Small parts for Metton LMR are in the 8 to 10 ft² (1 m²) range which is the upper end for cost and size capability for standard injection molding. In addition, Metton LMR parts do not require identical part geometry for multi-cavity molds.

Metton LMR is a family of lightly cross linked olefinic thermoset polymers based on polydicyclopentadiene (PDCPD) with mechanical property performance attributes similar to engineering thermoplastics. In the Metton LMR molding process, two low - viscosity DCPD liquid streams - one containing an activator (A Component) and the other a catalyst (B Component) - are impingement mixed at a 1:1 ratio and injected at near room temperature into a closed mold. The resulting exothermic reaction (heat generating) creates a fully polymerized part in less than 60 seconds. Button to button cycle times are generally 4 to 6 minutes depending upon size and geometry

Key Words: Metton LMR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 44.8 MPaASTM D638
Elongation at Yield 4.0 %ASTM D638
Tensile Modulus 1.98 GPaASTM D638
Flexural Yield Strength 74.5 MPa5% strain; ASTM D790
Flexural Modulus 2.01 GPaASTM D790
Poissons Ratio 0.39
Shear Modulus 0.712 GPaCalculated
Izod Impact, Notched 4.00 J/cmASTM D256
 0.534 J/cm
@Temperature -40.0 °C
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
@Thickness 3.17 mm
ASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Metton LMR M1534 Liquid Molding Resin
Metton LMR M1539 Liquid Molding Resin
Lubrizol Telene 1610 A/B & A/BK Dicyclopentadiene (DCPD)
Overview of materials for Polydicyclopentadiene (PDCPD)
Lubrizol Telene 1650 A/BK Dicyclopentadiene (DCPD)

PMET40 / 52925

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.