System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Envalior Pocan® B 4225 000000 PBT, 20% Glass Fiber
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Material Notes:
PBT, 20% glass fibers, injection molding, flame retardant
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.57
g/cc
ISO 1183
Water Absorption
0.30 %
Test Sim. to ISO 62
Moisture Absorption at Equilibrium
0.10 %
23°C/50% R.H.; Test Sim. to ISO 62
Viscosity Number
97
cm³/g
ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow
0.0049
cm/cm
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse
0.0018
cm/cm
ISO 294-4, 2577
Melt Flow
22
g/10 min
@Load 2.16 kg,
Temperature 260 °C
Calculated from MVR using melt density; ISO 1133
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
125
MPa
ISO 527-1/-2
Elongation at Break
2.5 %
ISO 527-1/-2
Tensile Modulus
8000
MPa
ISO 527-1/-2
Charpy Impact Unnotched
40.0
kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
40.0
kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched
<=
10.0
kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
<=
10.0
kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Impact
628
Puncture maximum force (N); ISO 6603-2
Puncture Energy
1.80
J
ISO 6603-2
Tensile Creep Modulus, 1 hour
7300
MPa
ISO 899-1
Tensile Creep Modulus, 1000 hours
6900
MPa
ISO 899-1
Electrical Properties
Original Value
Comments
Volume Resistivity
>=
1.00e+15
ohm-cm
IEC 60093
Surface Resistance
>=
1.00e+15
ohm
IEC 60093
Dielectric Constant
3.6
@Frequency 1e+6 Hz
IEC 60250
3.8
@Frequency 100 Hz
IEC 60250
Dielectric Strength
29.0
kV/mm
IEC 60243-1
Dissipation Factor
0.0040
@Frequency 100 Hz
IEC 60250
0.018
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
200
V
IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
30.0
µm/m-°C
ISO 11359-1/-2
CTE, linear, Transverse to Flow
120
µm/m-°C
ISO 11359-1/-2
Melting Point
225
°C
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)
220
°C
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
210
°C
ISO 75-1/-2
Deflection Temperature at 8.0 MPa
126
°C
ISO 75-1/-2
Vicat Softening Point
205
°C
50°C/h 50N; ISO 306
Flammability, UL94
V-2
@Thickness 0.800 mm
IEC 60695-11-10
V-0
@Thickness 1.60 mm
IEC 60695-11-10
5VA
@Thickness 3.50 mm
IEC 60695-11-20
Oxygen Index
32 %
ISO 4589-1/-2
Processing Properties
Original Value
Comments
Melt Temperature
260
°C
Injection Molding; ISO 294
Mold Temperature
80.0
°C
Injection Molding; ISO 10724
Descriptive Properties
Additives
Flame retarding agent
Lubricants
Features
Flame retardant
Form
Pellets
ISO Short Name
ISO 7792-1-PBT,GFHMR,09-080,GF20; ISO 1043-PBT GF FR(17)
Processing
Injection molding
Region
Asia Pacific
Europe
Near East/Africa
North America
South and Central America
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Celanese Crastin® SK603 BK851 PBT-GF20
Envalior Pocan® B 3235 901510 PBT, 30% Glass Fiber
Celanese Crastin® SK601 BK851 PBT-GF10
Celanese Celanex® 3300D PBT, 30% Glass Reinforced
BASF Ultradur® B 4300 G4 20% Glass Filled PBT
PLANX0861 / 99076
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.